MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
TIMET TIMETAL® 15-3 Titanium Alloy (Ti-15V-3Cr-3Sn-3Al); Aged at 496°C/8 hr
Categories: Metal; Nonferrous Metal; Titanium Alloy; Beta Titanium Alloy

Material Notes: High-Strength, Cold Formable Strip Alloy

Industry Specifications: USA Aerospace: AMS 4914A.

Features: Cold formable and weldable, this strip alloy is primarily used for aircraft ducting, pressure vessels and other fabricated sheet metal structures up to 300°C.

Typical heat treatment for this alloy: Solution Treatment: 790°C for 3-20 min, air cool. Age Treatment: 480-620°C for 4-16 hrs.

Data provided by TIMET.

Key Words: 15-3-3-3
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 4.78 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate >= 1172 MPaspecified minimum for strip
Tensile Strength, Yield >= 1103 MPa
@Strain 0.2 %
specified minimum for strip
Elongation at Break >= 5.0 %specified minimum for strip
Modulus of Elasticity 109 GPa
 
Thermal PropertiesOriginal ValueComments
CTE, linear 4.70 µin/in-°F
@Temperature 22.8 - 93.3 °C
 5.20 µin/in-°F
@Temperature 22.8 - 316 °C
 5.50 µin/in-°F
@Temperature 22.8 - 538 °C
 6.10 µin/in-°F
@Temperature 22.8 - 760 °C
 8.60 µm/m-°C
@Temperature 20.0 °C
 9.20 µm/m-°C
@Temperature 20.0 - 250 °C
 9.90 µm/m-°C
@Temperature 20.0 - 500 °C
Specific Heat Capacity 0.500 J/g-°C
 0.120 BTU/lb-°F
@Temperature 22.8 °C
 0.130 BTU/lb-°F
@Temperature 204 °C
 0.160 BTU/lb-°F
@Temperature 538 °C
 0.190 BTU/lb-°F
@Temperature 760 °C
Thermal Conductivity 8.30 W/m-K
 60.0 BTU-in/hr-ft²-°F
@Temperature 22.8 °C
 74.0 BTU-in/hr-ft²-°F
@Temperature 204 °C
 110 BTU-in/hr-ft²-°F
@Temperature 538 °C
 138 BTU-in/hr-ft²-°F
@Temperature 760 °C
Maximum Service Temperature, Air 288 °C
Beta Transus 760 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 2.5 - 3.5 %
Carbon, C <= 0.050 %
Chromium, Cr 2.5 - 3.5 %
Hydrogen, H <= 0.015 %
Iron, Fe <= 0.25 %
Nitrogen, N <= 0.050 %
Other, each <= 0.10 %
Other, total <= 0.40 %
Oxygen, O <= 0.13 %
Tin, Sn 2.5 - 3.5 %
Titanium, Ti 72.6 - 78.5 %Calculated as remainder
Vanadium, V 14 - 16 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
TIMET TIMETAL® 15-3 Titanium Alloy (Ti-15V-3Cr-3Sn-3Al); Aged at 482°C/16 hr
TIMET TIMETAL® 15-3 Titanium Alloy (Ti-15V-3Cr-3Sn-3Al); Aged at 538°C/8 hr.
TIMET TIMETAL® 10-2-3 Titanium Alloy (Ti-10V-2Fe-3Al), Solution Treated and Aged 950°F (510°C)
AISI E4340 Steel, oil quenched 800°C (1470°F), 540°C (1000°F) temper, 13 mm (0.5 in.) round
TIMET TIMETAL® 15-3 Titanium Alloy (Ti-15V-3Cr-3Sn-3Al); Casting

NTIME153C / 200042

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.