Produced without animal derived components Sterilization: EtO and autoclave Applications: Nutritional drink bottles, pharmaceutical BFS, irrigation containers, and medical device components Regulatory: FDA – 21 CFR 177.1520(c) 3.2a; USP <88> Class VI, USP<85>, and ISO 10993-5 Information provided by INVISTA. |