MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SABIC BC 112 Crystalline Polyethylene Terephthalate  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), Unreinforced

Material Notes: BC 112 is a crystalline, high molecular weight thermoplastic polymer made by a continuous melt-phase polymerization process followed by solid-state polymerization.

Characteristics: BC 112 is a specially formulated bottle grade PET that is characterized by High I.V. and low acetaldehyde. The High I.V. confers good mechanical properties; high burst strength s and reduced bottle distension after filling.

Typical Applications: BC 112 is especially suitable for the production of bottles for carbonated drinks. The high I.V. gives the bottle extra mechanical strength required in hot climates due to the high pressures from carbonation. It can also be used for bottles for noncarbonated (except water) and other packaging applications, e.g., edible oil & thermoformed packaging.

Information provided by SABIC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.828 - 0.848 g/ccASTM D1895
Density <= 1.39 g/cccrystalline density; SABIC (IRC0032)
Viscosity Test 82 - 86 cm³/gIntrinsic; SABIC (IRC0041)
Maximum Moisture Content <= 0.35% w/w; SABIC (IRC0050)
 
Chemical PropertiesOriginal ValueComments
Acetaldehyde <= 1.00 ppmSABIC (IRC0057
 
Thermal PropertiesOriginal ValueComments
Melting Point 246 - 256 °CSABIC (IRC0053)
 
Descriptive Properties
Color (b)-1.5 ± 2.0
Color (L)89 ± 4.0
DEG Content< 1.5 % w/wSABIC (IRC0055)
Dust Content< 0.01 % w/wSABIC (IRC0060)

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DAK Americas Laser+® MB912 PET
SABIC BC 110 Crystalline Polyethylene Terephthalate
BLUESTAR PBT 6630 30% Glass Filled
Dow LIGHTER™ S98 Polyethylene Terephthalate (PET) Resin
Plastcom SLOVASTER® B GF 30 Polybutylene Terephthalate, 30% Glass Fiber

PSABICZ845 / 133041

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.