MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Wellman EcoLene™ PP8002-BK1 Polypropylene with 30% Glass Fiber Filler
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 30% Glass Fiber Filler

Material Notes: Wellman Advanced Materials via its Post-Consumer, EcoLene™ Product Line, has been a key participant in the automotive industry’s recent shift towards “green” manufacturing. Being composed of 100% Post-Consumer Recycled Materials, EcoLene™ products are eco-friendly while still maintaining quality. Building on Wellman Advanced Materials’ recycling strength and its our EcoLon™ product line; our EcoLene™ Post-Consumer Recycled (PCR) Polypropylene Line, is gaining ground in the Industry. This product line provides a more, eco-friendly alternative to virgin polypropylene. Applications: Engine covers, Door Modules, Battery Trays, Gun Stocks, Sprinkler System.

Information provided by Wellman Advanced Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.16 g/cc0.0419 lb/in³ISO 1183
Filler Content 30 %30 %Glass; ISO 3451
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 84.0 MPa12200 psiISO 527
Elongation at Break 3.0 %3.0 %ISO 527
Flexural Strength 125 MPa18100 psiISO 178
Flexural Modulus 6.117 GPa887.2 ksiISO 178
Charpy Impact, Notched 0.740 J/cm²3.52 ft-lb/in²ISO 180
 
Thermal PropertiesMetricEnglishComments
Melting Point 160 °C320 °FISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 140 °C284 °FISO 75
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 216 - 243 °C421 - 469 °F
Middle Barrel Temperature 216 - 243 °C421 - 469 °F
Front Barrel Temperature 221 - 249 °C430 - 480 °F
Nozzle Temperature 221 - 249 °C430 - 480 °F
Mold Temperature 33.0 - 66.0 °C91.4 - 151 °F
Injection Pressure 69.0 - 103 MPa10000 - 14900 psi
Back Pressure 0.340 - 1.03 MPa49.3 - 149 psi
Screw Speed 30 - 100 rpm30 - 100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PWEL00840 / 249964

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.