MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Saint-Gobain CHR® 2905-7R Glass Cloth Backing Silicone Adhesive Pressure Sensitive Tape
Categories: Polymer; Adhesive; Tape; Thermoset; Silicone

Material Notes: CHR® 2905 is manufactured from heat-resistant fibreglass cloth backing coated with high-temperature silicone adhesive on both sides.

Features/Benefits: CHR® 2905 is exceptionally stable at high temperatures, allowing it to withstand temperatures up to 260 °C. A non-corrosive product, 2905 is used in a variety of critical electrical applications. Other characteristics include excellent abrasion and edge tear resistance and exceptional flex strength. CHR® 2905 is available in both 0.178 mm and 0.254 mm thicknesses, the 0.254 mm (2905-10R) being a more abrasive-resistant, heavy-duty product.

Applications: CHR® 2905 has a wide variety of uses in the industrial and electrical markets. It is most widely used as a high temperature masking tape for metalising or plasma spray coatings. CHR® 2905 is also used as a holding tape for components on circuit boards, inner wraps for coils and transformers and high temperature splicing.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Elongation at Break <= 10 %<= 10 %
Tear Strength 30.7 kN/m175 pliTensile Strength
Peel Strength 0.440 kN/m2.51 pliAdhesion to Steel
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 260 °C500 °F
Minimum Service Temperature, Air -73.0 °C-99.4 °F
 
Descriptive Properties
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Saint-Gobain CHR® 2915-7 Glass Cloth Backing Silicone Adhesive Pressure Sensitive Tape
Saint-Gobain CHR® 2905-10R Glass Cloth Backing Silicone Adhesive Pressure Sensitive Tape

PSTGQZ375 / 68889

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.