MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Mitsubishi Chemical Advanced Materials TIVAR® Burnguard Flame Retardant Lining Material (ASTM Product Data Sheet)  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); UHMW PE (Ultra High Molecular Weight PE)

Material Notes: TIVAR® 88 w/ BurnGuard Ultra High Molecular Weight Polyethylene UHMW-PE / TIVAR® Burnguard Ultra High Molecular Weight Polyethylene UHMW-PE static dissipative and flame retardant shapes, were specifically developed to improve the flammability behavior of unfilled polyethylene grades. This grade in particular possesses a UL94 V-0 Flammability Rating, and also meets MSHA 1C-112/1 requirements for underground mining. Due to these characteristics, TIVAR® 88 w/BurnGuard UHMW-PE / TIVAR® Burnguard UHMW-PE excels in applications where key components may be exposed to combustion such as bunker and chute liners, hopper liners, railcar liners, self-unloading ships, railcar liners, dragline buckets, belt scrapers, storage bin liners, vibratory feeder liners, and wear strips.

  • Promotes reliable, steady bulk material flow
  • Abrasion-, chemical- and corrosion-resistant
  • Low coefficient of friction
  • No moisture absorption
  • Reduces or eliminates arching, ratholing and erractic flow

Quadrant Engineering Plastic Products is now Mitsubishi Chemical Advanced Materials.

Key Words: TIVAR® 88 W/BurnGuard
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.00 g/ccASTM D792
Water Absorption <= 0.010 %Immersion, 24hr; ASTM D570(2)
Water Absorption at Saturation <= 0.010 %Immersion; ASTM D570(2)
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 64ASTM D2240
Tensile Strength 3600 psiASTM D638
Tensile Strength at 65°C (150°F) 400 psiASTM D638
Elongation at Break 120 %ASTM D638
Tensile Modulus 87.0 ksiASTM D638
Flexural Strength 2900 psiASTM D790
Flexural Modulus 94.0 ksiASTM D790
Compressive Strength 2800 psi10% Def.; ASTM D695
Compressive Modulus 65000 psiASTM D695
Izod Impact, Notched NBASTM D256 Type A
Coefficient of Friction, Dynamic 0.090Dry vs. Steel; QTM55007
Sand Slurry 151018 Steel = 100
Limiting Pressure Velocity 4000 psi-ft/min4:1 safety factor; QTM 55007
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square >= 1.00e+12 ohmASTM D257
 
Thermal PropertiesOriginal ValueComments
CTE, linear 90.0 µin/in-°F
@Temperature -40.0 - 149 °C
ASTM E831
Melting Point 275 °FCrystalline, Peak; ASTM D3418
Maximum Service Temperature, Air 180 °FLong Term
Deflection Temperature at 1.8 MPa (264 psi) 116 °FASTM D648
Flammability, UL94 V-0
@Thickness 3.17 mm
Estimated Rating
 
Compliance PropertiesOriginal ValueComments
3A-Dairy No
Canada AG No
FDA No
NSF No
USDA No
USP Class VI No
 
Chemical Resistance PropertiesOriginal ValueComments
Acids, Strong (pH 1-3) Limited
Acids, Weak Acceptable
Alcohols Acceptable
Alkalies, Strong (pH 11-14) Acceptable
Alkalies, Weak Acceptable
Chlorinated Solvents Acceptable
Conductive / Static Dissipative Yes
Continuous Sunlight Limited
Hot Water / Steam Limited
Hydrocarbons - Aliphatic Acceptable
Hydrocarbons - Aromatic Unacceptable
Inorganic Salt Solutions Acceptable
Ketones, Esters Limited
 
Descriptive Properties
Machinability31-10, 1=Easier to Machine

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
PTS Trilac® ABS-HF5500 High Flow ABS Resin
PTS Trilac® FR3800-V Flame Retardant ABS Resin, RoHS Compliant
Mitsubishi Chemical Advanced Materials TIVAR™ 88-2 ESD UHMW-PE Black, Premium Lubricant Filled, Lower COF, Electro Static Dissipative Lining Material
Mitsubishi Chemical Advanced Materials TIVAR™ 88-2 UHMW-PE, Premium Lubricant Filled Lining Material
Mitsubishi Chemical Advanced Materials TIVAR™ 1000 Virgin UHMW-PE, (Natural & Colors except Black)

P1SMP09 / 20159

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.