UL94 V-0, flame retarded, high impact polystyrene. This grade is suitable for injection moulding. It combines high mechanical strength, heat resistance and good processability.
Designation: Thermoplastics ISO 2897-PS-I,M,093-06-04-18 Applications: Typical applications are in the field of TV back covers, structural parts forbusiness machines, painted moulded items for electronics. The natural version is certified UL94 V-0 at 2.2 mm (UL file E83071). This grade may be supplied in natural or colored version upon request. Information provided by Polimeri Europa Versalis is the Eni subsidiary containing the plastics and rubber businesses. |