MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ATI Allvac® Nickelvac® 901 Nickel Superalloy, Heat Treatment: 1010°C (1850°F) + Age  (discontinued **)
Categories: Metal; Nonferrous Metal; Nickel Alloy; Superalloy

Material Notes: Data provided by Allvac.

Applications: Turbine discs and shafts, compressor blades and discs, high-temperature bolting, high-temperature devices, cryogenics.

Key Words: Allvac, an Allegheny Teledyne Company, UNS N09901; AMS 5660, 5661
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 8.22 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 334Estimated from Rockwell C value for Brinell test with 3000 kg load/10 mm diameter ball
Hardness, Knoop 363Estimated from Rockwell C value.
Hardness, Rockwell C 36
Hardness, Vickers 349Estimated from Rockwell C value.
Tensile Strength, Ultimate 1276 MPa
Tensile Strength, Yield 1172 MPa
@Strain 0.2 %
Elongation at Break 25 %
Reduction of Area 40 %
 
Component Elements PropertiesOriginal ValueComments
Boron, B 0.015 %
Carbon, C 0.050 %
Chromium, Cr 12.5 %
Iron, Fe 36 %as balance
Molybdenum, Mo 6.0 %
Nickel, Ni 43 %
Titanium, Ti 2.8 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ATI Allegheny Ludlum AL 600™ Nickel-Base Alloy, UNS N06600
ATI Allvac® Astroloy Nickel Superalloy, Heat Treatment: 1163°C (2125°F) + Age
Incoloy 901, RGT 8, Fe-PA 99-Ht, (UNS N09901) Superalloy
ATI Allvac® Nickelvac® 600 Nickel Superalloy, Heat Treatment: 927°C (1700°F) Anneal
ATI Allvac® Nickelvac® 800-H Nickel Superalloy (UNS N08810)

NALL13 / 14781

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.