MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Danquinsa MORCHEM UD 5037F Polyurethane dispersion
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: MORCHEM UD 5037F is an anionic, aliphatic structured polyester based polyurethane dispersion. This polyurethane dispersion distinguish itself by its elastic film hardness in the range of shore hardness 75-77A. This PU dispersion based on aliphatic distinguish itself by the excellent UV constancy and is the element raw material for producing divers aqueous polyurethane adhesives, adhesive coatings and adhesive equipment. This dispersion is also used as a lamination coating and as Top Coat in the textile coating. Furthermore this dispersion is also suitable for producing of leather finishes and leather covering color.

Application: MORCHEM UD 5037F is applied to serve as a basic raw material by the production of aqueous 1- and 2-component adhesives. Adhesives and adhesive coatings which were produced with MORCHEM UD 5037F are especially good suitable for:

  • Textile lamination
  • Coating of casings and profiles
  • Lamination of thermoplastic foils with wooden materials as for instance by membrane press application
  • Deep-draw and press lamination application for the automotive industry.
  • Shoe soles- and shoe shank fitting
  • Lamination of split leather and plastic foils. We recommend, for the processing of 2- component adhesives, the application of the cross link agent DANCURE 101.

Information provided by Danquinsa GMBH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 39 - 41 %39 - 41 %
pH 7.0 - 9.07.0 - 9.0
Viscosity 150 cP150 cP
Storage Temperature 5.00 - 25.0 °C41.0 - 77.0 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 32.0 MPa4640 psiDIN 53.504
Elongation at Break 680 %680 %DIN 53.504
100% Modulus 4.80 MPa696 psiDIN 53.504
300% Modulus 8.00 MPa1160 psiDIN 53.504
 
Processing PropertiesMetricEnglishComments
Shelf Life 6.00 Month6.00 Month
 
Descriptive Properties
AspectLow viscose, white liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDANQ186 / 294606

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.