MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Nylene® Nylene 615 NP Nylon 6, Extruded
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Extruded

Material Notes: Nylon 6 polymer designed for use in extrusion of tubing and film to be used in food packaging. High melt strength for shape retention. Like most PA6, Nylene 615 NP has excellent grease resistance, toughness, and resistance to abrasion.

Testing conducted on dry as molded specimen at 73°F

Information provided by Nylene® Global Polymer Solutions.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.13 g/cc1.13 g/ccASTM D792
Viscosity Test 250 cm³/g2.50 dl/g
Permeability 3.13.1Oxygen, cc-mil/ 24hr-atm
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, TD 300 %300 %ASTM D882
Secant Modulus, TD 0.648 GPa94.0 ksiASTM D882
Elmendorf Tear Strength, TD 2.17 g/micron55.0 g/milASTM D789
Film Tensile Strength at Break, TD 68.9 MPa10000 psiASTM D638
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 °C428 °FASTM D3418
 
Descriptive Properties
Yield Stress24500 in2/lbASTM D638

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNYLEN919 / 221451

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.