MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Sumitomo Bakelite NEONIT® SK61 L5G Epoxy Molding Compound
Categories: Polymer; Thermoset; Epoxy; Epoxy Molding Compound

Material Notes: NEONIT® SK61 L5G is a long glass fiber reinforced epoxy molding compound with excellent long term property retention over a wide temperature range and climate conditions. It is particularly suited for over molding.

Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.80 g/cc0.0650 lb/in³ISO 1183
Apparent Bulk Density 0.650 g/cc0.0235 lb/in³ISO 60
Water Absorption 0.060 %0.060 %ISO 62
Linear Mold Shrinkage 0.0015 cm/cm0.0015 in/inISO 2577
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 115 MPa16700 psiISO 527-1
Elongation at Break 0.80 %0.80 %ISO 527-1
Tensile Modulus 18.0 GPa2610 ksiISO 527-1
Flexural Strength 215 MPa31200 psiISO 178
Flexural Modulus 16.0 GPa2320 ksiISO 178
Compressive Strength 248 MPa36000 psiISO 604
Charpy Impact, Notched 5.10 J/cm²24.3 ft-lb/in²ISO 179-1
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 30.0 kV/mm762 kV/inIEC 60243-1
Comparative Tracking Index 600 V600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 10.0 µm/m-°C5.56 µin/in-°FTMA
CTE, linear, Transverse to Flow 53.0 µm/m-°C29.4 µin/in-°FTMA
Glass Transition Temp, Tg 150 °C302 °FTMA
Shrinkage -0.0200 %-0.0200 %Post; ISO 2577
 
Descriptive Properties
ColorDark Grey

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sumitomo Bakelite NEONIT® K82 L8 Epoxy Molding Compound
Sumitomo Bakelite NEONIT® K600 Fe Epoxy Molding Compound
Raschig Group EPOXIDUR® 3580 EP Epoxy
Raschig Group 3581 Epoxy
Park Aerospace Nelco® N4000-12 High Speed/Low Loss, CAF Resistant Laminate and Prepreg

PSUMIT176 / 193981

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.