MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Lucas-Milhaupt HI-TEMP® 910 Nickel-Silicon-Boron-Iron Brazing Alloy (AWS BNi-3)
Categories: Metal; Nonferrous Metal; Nickel Alloy; Solder/Braze Alloy

Material Notes: Hi-Temp 910 is a nickel -silicon-boron-iron brazing alloy powder with low joining temperature. It provides high temperature joint strength plus oxidation, corrosion, and abrasion resistance on thick sections of stainless steel, ductile nickel, and cobalt base alloys. Typical applications would include structural members in jet engines, turbines, chemical processing, and nuclear equipment (not exposed to radiation) requiring lower brazing/heat treatment temperatures. Hi-Temp 910 will flow into long, narrow joints, in marginal atmospheres but will flow particularly well at the higher brazing temperature, in reducing atmospheres (-60°F dew point or lower) or inert atmospheres (-80°F dew point or lower).

Available forms: Powder and paste. Available mesh sizes for powder.

Information provided by Lucas-Milhaupt.

Key Words: SAE/AMS 4788
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 7.33 g/cc7.33 g/cc
Density 7.34 g/cc0.265 lb/in³
 
Thermal PropertiesMetricEnglishComments
Melting Point 982 - 1040 °C1800 - 1900 °F
Solidus 982 °C1800 °F
Liquidus 1040 °C1900 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 1010 - 1180 °C1850 - 2150 °FBrazing Range
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al <= 0.050 %<= 0.050 %
Boron, B 2.75 - 3.5 %2.75 - 3.5 %
Carbon, C <= 0.060 %<= 0.060 %
Cobalt, Co <= 0.10 %<= 0.10 %
Iron, Fe <= 0.50 %<= 0.50 %
Nickel, Ni 90.2 - 91.9 %90.2 - 91.9 %Remainder
Other, total <= 0.50 %<= 0.50 %
Phosphorus, P <= 0.020 %<= 0.020 %
Selenium, Se <= 0.0050 %<= 0.0050 %
Silicon, Si 4.0 - 5.0 %4.0 - 5.0 %
Sulfur, S <= 0.020 %<= 0.020 %
Titanium, Ti <= 0.050 %<= 0.050 %
Zirconium, Zr <= 0.050 %<= 0.050 %
 
Descriptive Properties
ColorIron Gray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

NLUCM9824 / 254770

solder replacement adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.