Sequel 1440-UV WA3 BLACK engineered polyolefin material is typically used for large automotive exterior applications that require ductile impact properties at low temperatures, has excellent part appearance and processability. Applications: Bumpers, Exterior Automotive ApplicationsInformation provided by LyondellBasell. |