MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

3M VHB™ F9473PC Adhesive Transfer Tapes with Adhesive 100MP
Categories: Polymer; Adhesive

Material Notes: 3M™ VHB™ Adhesive Transfer Tapes F9460PC, F9469PC and F9473PC utilize the 3M™ High Performance Acrylic Adhesive 100MP, which has excellent long term holding power with much higher adhesion strength than typical pressure sensitive adhesive systems. These 3M™ VHB™ Adhesive Transfer Tapes are transparent and are ideal for use in many interior and exterior industrial applications to replace rivets, spot welds, liquid adhesives, and other permanent fasteners.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.980 g/cc0.0354 lb/in³
Thickness 102 microns4.00 milLiner Material
 254 microns10.0 milAdhesive
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 0.690 MPa100 psiT-Block on Aluminum; ASTM D987
Shear Strength 0.552 MPa80.0 psiDynamic Shear to Stainless Steel; ASTM D1002
Peel Strength 1.58 kN/m9.00 plito Stainless Steel; ASTM D3330
 
Electrical PropertiesMetricEnglishComments
Insulation Resistance >= 1.00e+6 ohm>= 1.00e+6 ohmASTM D1000
Dielectric Strength  39.4 kV/mm
@Temperature 125 °C
1000 kV/in
@Temperature 257 °F
ASTM D149-97A
 39.4 kV/mm
@Temperature 175 °C
1000 kV/in
@Temperature 347 °F
ASTM D149-97A
 47.2 kV/mm
@Temperature 23.0 °C
1200 kV/in
@Temperature 73.4 °F
ASTM D149-97A
 74.8 kV/mm
@Temperature 175 °C
1900 kV/in
@Temperature 347 °F
ASTM D149-97A
 102 kV/mm
@Temperature 125 °C
2600 kV/in
@Temperature 257 °F
ASTM D149-97A
 118 kV/mm
@Temperature 23.0 °C
3000 kV/in
@Temperature 73.4 °F
ASTM D149-97A
 217 kV/mm
@Temperature 23.0 °C
5500 kV/in
@Temperature 73.4 °F
ASTM D149-97A
 
Thermal PropertiesMetricEnglishComments
CTE, linear 77.0 µm/m-°C42.8 µin/in-°F
Thermal Conductivity 0.669 W/m-K4.64 BTU-in/hr-ft²-°FASTM C177
Maximum Service Temperature, Air 149 °C300 °FLong Term
 260 °C500 °FShort Term
 
Processing PropertiesMetricEnglishComments
Shelf Life 18.0 Month18.0 Month
 
Descriptive Properties
Liner58# polycoated Kraft

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M VHB™ F9460PC Adhesive Transfer Tapes with Adhesive 100MP
3M VHB™ F9469PC Adhesive Transfer Tapes with Adhesive 100MP
3M 9453FL Adhesive Transfer Tape with 300LSE Adhesive
Silver, Ag
3M 9472FL Adhesive Transfer Tape with 300LSE Adhesive

PMM33338 / 168085

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.