MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Reynolds PMC® 746 Polyurethane Rubber Compound
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Elastomer, Unreinforced

Material Notes: Product Overview: PMC®-746 was developed to make molds for casting gypsum plasters. Like PMC®-744, this product is well suited for use as a rubber case mold – especially large case molds where extra rigidity is required. Shore hardness is 60A. Because of its durability and moisture resistant properties PMC®-746 is also used by zoos and museums for a variety of mold-making, display and exhibit applications. It features a convenient mix ratio (2:1 by weight or volume), and contains no mercury. Other applications include making plaster block molds, reproducing ornamental plaster (architectural restoration), pre-cast concrete molds, casting waxes, Smooth-On rigid polyurethanes and epoxies and also for making a variety of special effects for movies and theatre.

Information provided by Reynolds Advanced Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.03 g/cc1.03 g/ccASTM D-1475
Viscosity 1200 cP1200 cPMixed; ASTM D-2393
Linear Mold Shrinkage <= 0.0010 cm/cm<= 0.0010 in/in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6060ASTM D-2240
Tensile Strength 4.83 MPa700 psiASTM D-412
Elongation at Break 650 %650 %ASTM D-412
100% Modulus 1.52 MPa220 psiASTM D-412
Tear Strength 17.5 kN/m100 pliDie C; ASTM D-624
 
Processing PropertiesMetricEnglishComments
Cure Time 960 min16.0 hour
Pot Life 15.0 min15.0 minASTM D-2471
 
Descriptive Properties
ColorAmber
Mix Ratio2A:1Bby volume
 2A:1Bby weight
Specific Volume26.9[cu. in./lb.]

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PREYN078 / 296779

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.