MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Eastman TMPD™ Glycol
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: CAS No. 144-19-4

Product Description: Eastman TMPD™ glycol is used to formulate saturated polyester resins for liquid coatings and unsaturated polyester laminating resins. Markets for Eastman TMPD™ glycol include metal office furniture, automotive, industrial maintenance, general metal, and fiberglass-reinforced plastics for composites. Eastman TMPD™ glycol can be shipped in bags in white, waxy platelet form, cast solid form in drums, or in bulk molten form in tank trucks.

Application/Uses:

  • Appliances
  • Automotive refinish
  • Coatings
  • Coatings for automotive
  • Cosmetic polymer intermediate
  • High solid coatings
  • Thermoset resin FRP
  • Waterborne coatings
Key Attributes:
  • Allows the formulation of very stable waterborne polyesters
  • Excellent chemical, stain, humidity, and corrosion resistance properties
  • Ideal for formulating high-solids, low VOC coatings
  • Low viscosity and density with excellent solubility in solvents
  • Outstanding corrosion resistance in fiberglass-reinforced plastics

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.688 g/cc0.0249 lb/in³Granulated
 0.897 g/cc0.0324 lb/in³Solid Cake
 0.928 g/cc0.0335 lb/in³
Molecular Weight 146.22 g/mol146.22 g/mol
 
Thermal PropertiesMetricEnglishComments
Melting Point 46.0 - 55.0 °C115 - 131 °F
Boiling Point 220 °C428 °FInitial
 235 °C455 °F95%
Flash Point 113 °C235 °FCleveland Open Cup
 
Descriptive Properties
ColorPt-Co, Molten
Fire Point118Cleveland Open Cup

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEATM5184 / 222378

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.