MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Emerald Performance Materials Hypro™ 1300X31 CTBN Carboxyl-Terminated Butadiene-Acrylonitrile
Categories: Polymer; Thermoset

Material Notes: Copolymer with 10% acrylonitrile, increased compatibility with filled systems.

Information provided by Emerald Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.924 g/cc0.924 g/cc
Viscosity 65000 cP65000 cP
Molecular Weight 3800 g/mol3800 g/mol
 
Chemical PropertiesMetricEnglishComments
Total Acid Number 3030[mgKOH/g]
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg -66.0 °C-86.8 °F
 
Optical PropertiesMetricEnglishComments
Gardner Color Number 5.05.0
 
Descriptive Properties
Acrylonitrile10 percent
Carboxyl Equiv0.05 phr
Functionality1.9
Solubility Parameter8.46 cal/cm3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sumitomo Bakelite Durez® 118 Phenolic, Compression Grade
DuPont™ Kevlar® 49 Aramid Fiber
Dow Elvax® 250 Ethylene-Vinyl Acetate Copolymer Resin
Emerald Performance Materials Hypro™ 1300X9 CTBNX Carboxyl-Terminated Butadiene-Acrylonitrile

PEMERA861 / 209689

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.