MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

AlphaGary Garaflex™ G 7795-A7 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Garaflex™ G is a thermoplastic elastomer intended for wire and cable applications
125°C rated flame retardant TPE for appliance and automotive wiring.

Alphagary is part of Orbia.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 44 - 4844 - 48
Tensile Strength 17.2 MPa2500 psi
Elongation at Break 550 %550 %ASTM D412
 
Thermal PropertiesMetricEnglishComments
Oxygen Index 30 %30 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3D Systems LaserForm™ A6 Tool Steel Powder for Rapid Tooling and Rapid Manufacturing
AISI Type W1 Tool Steel, water quenched at 775°C (1425°F), tempered 350°C (660°F)
AISI Type W1 Tool Steel, austenitized at 785-815°C (1450-1500°F)
AISI Type A7 Tool Steel
MetalTek MTEK A6 Tool Steel

PGARY9882 / 140668

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.