MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

BASF Adipic Acid
Categories: Fluid

Material Notes: Recommended use: For the production of homopolymerisates and copolymerisates, initial product for chemical syntheses

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.700 g/cc0.0253 lb/in³
Density 1.36 g/cc0.0491 lb/in³
Solubility in Water 2.3 %2.3 %
pH 2.72.7100 g/l
Molecular Weight 146.14 g/mol146.14 g/mol
Vapor Pressure 0.0000970 bar
@Temperature 25.0 °C
0.0728 torr
@Temperature 77.0 °F
 
Thermal PropertiesMetricEnglishComments
Melting Point 150.85 °C303.53 °F
Boiling Point 337.5 °C
@Pressure 0.1031 MPa
639.5 °F
@Pressure 14.96 psi
Flash Point >= 196 °C>= 385 °F
Ignition Temperature 405 °C761 °FDIN 51794
 
Descriptive Properties
ColorWhite
Commercial StatusEurope
Minimum Ignition energy1 bar; VDI 2263, sheet 1, 2.5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil PP5722E1 Polypropylene Copolymer
Bamberger Polymers Bapolene® 5083C Polypropylene, Injection Grade
Bamberger Polymers Bapolene® 5072 Polypropylene, Injection Grade
Bamberger Polymers Bapolene® 5065NB Polypropylene Impact Copolymer
Bamberger Polymers Bapolene® 5063C Polypropylene, Injection Grade

PBASG0211 / 131844

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.