MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Tabriz HS221 Performance Expandable Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Expanded Polystyrene (EPS)

Material Notes: HS221 is a free flowing expandable polystyrene grade, consisting of spherical polystyrene beads containing pentane as the expansion agent. Expandable polystyrene (EPS) is normally expanded to achieve the low densities required for final step expansion. The typical density of this grade is around 22 kg/m3, but other densities are possible depending on applications and equipments. HS221 is specially high strength formulated to achieve low density foam without lumps during preexpansion. This grade is not fire retardant so it is not suitable for building applications. Applications: Medium Density Block. Low- and medium-density foam blocks made from HS 221 are used as thermal insulation boards for construction applications without special requirements concerning flame resistance or as packaging blanks.

Information provided by Tabriz Petrochemical Commercial Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.0140 - 0.0300 g/ccExpanded; SUNPOR 7 2.6
Bead Size 1.00 - 1.80 mm>90% WT; SUNPOR 7 2.5 (MIN 90% BY WT)
 
Descriptive Properties
K-Value55SUNPOR 7 2.4
Pentane Content (wt%)5.2SUNPOR 7 2.2
Styrene Residual Monomer500 ppmSUNPOR 7 2.1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
NOVA Chemicals Arcel 730 70% PS/30% PE Interpolymer
Jackon JACKOCELL® R311 Expanded Polystyrene Packaging and Shape Molding
Tabriz HS121 Expandable Polystyrene
Jackon JACKOCELL® S332 Expanded Polystyrene Packaging and Shape Molding
NOVA Chemicals ARCEL® 730B Expanded Polyethylene/Styrenic Polymer

PIPC091 / 48319

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.