MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Kazanorgsintez PE2NT22-12 High Density Polyethylene Composite
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Injection Molded

Material Notes: Production Method: Copolymerization of eythylene at low pressure in presence of complex catalysts using gaseous-phase method.

Application: Composition is intended for injection molding processing into goods for household and domestic use or for other field of application and characterized by advanced crack resistance.

Information Provided by Kazanorgsintez

Key Words: HDPE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.958 - 0.965 g/cc
@Temperature 23.0 °C
 0.960 - 0.966 g/cc
@Temperature 20.0 °C
Melt Flow 6.0 - 9.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
±15%
 120 - 315 g/10 min
@Load 21.6 kg,
Temperature 190 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield >= 28.0 MPa
Elongation at Break >= 500 %
 
Descriptive Properties
Amount of impurities [pcs]10

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
NIZHNEKAMSKNEFTEKHIM PE 2060S (60105) High Density Polyethylene
NIZHNEKAMSKNEFTEKHIM PE 4050Q (50403) High Density Polyethylene
Chevron Phillips HiD® 9062 HDPE Injection Molding Resin
Chevron Phillips HiD® 9055 HDPE Injection Molding Resin
Chevron Phillips Marlex® 9004 HDPE Injection Molding Resin

PKAZAN011 / 127330

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.