MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Parker Chomerics CHO-SEAL® 6435 Conductive Elastomer
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Silicone

Material Notes: Description: Material of choice for high shielding effectiveness where NBC fluid resistance is needed; good performance in corrosive environments.

Molded only

RoHS Compliant

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 3.45 - 3.95 g/cc3.45 - 3.95 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 73 - 8773 - 87ASTM D2240
Tensile Strength >= 1.38 MPa>= 200 psiASTM D412
Elongation at Break <= 200 %<= 200 %ASTM D412
Tear Strength <= 13.1 kN/m<= 75.0 pliASTM D624
Compression Set <= 40 %
@Temperature 100 °C,
Time 252000 sec
<= 40 %
@Temperature 212 °F,
Time 70.0 hour
ASTM D395, Method B
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 0.0060 ohm-cm<= 0.0060 ohm-cmwithout pressure-sensitive adhesive; CEPS-0002
Shielding Effectiveness  >= 85 dB
@Frequency 2.00e+9 Hz
>= 85 dB
@Frequency 2.00e+9 Hz
Plane Wave; Method 2, MIL-DTL-83528 Para. 4.6.12
 >= 85 dB
@Frequency 1e+10 Hz
>= 85 dB
@Frequency 1e+10 Hz
Plane Wave; Method 2, MIL-DTL-83528 Para. 4.6.12
 >= 100 dB
@Frequency 5.00e+8 Hz
>= 100 dB
@Frequency 5.00e+8 Hz
E-Field; Method 2, MIL-DTL-83528 Para. 4.6.12
 >= 105 dB
@Frequency 1e+8 Hz
>= 105 dB
@Frequency 1e+8 Hz
E-Field; Method 2, MIL-DTL-83528 Para. 4.6.12
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 1.80 W/m-K
@Pressure 2.07 MPa
12.5 BTU-in/hr-ft²-°F
@Pressure 300 psi
ASTM D5470
Maximum Service Temperature, Air 100 °C212 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °FFlex TR10
 
Descriptive Properties
BinderEPDM
FillerAg/Ni
Heat Aging<0.0125 ohm-cm100°C for 48hrs; CEPS-0002

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Vicone High Performance Rubber VicoSeal™ 07EK-BK High Performance EPDM Rubber
Dow Nordel® IP 4520 General Purpose Molding
Mocom (ALBIS) Alfater XL® A30I 4GP0000 Thermoplastic Vulcanizate PP/EPDM-Elastomer
ATG s.r.l. EPDM Ethylene-Propylene Terpolymer
Dow Nordel® IP 4520 Molded Golf Grip

PCHOME225 / 130935

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.