MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Thermal Ceramics Kaowool 2600 High Temperature Board
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: Kaowool 2600 using high alumina fibers along with Kaowool ceramic fibers is an excellent dimensional stable product at 2600°F (1427°C) where minimal shrinkages are very important.

Applications:

  • Appliance and heat processing
  • Backup insulation to dense refractories
  • Bullnose tiles
  • Burner blocks
  • Combustion chamber construction
  • Expansion joint material
  • Flue and chimney linings
  • Furnace components
  • Furnace door linings
  • Furnace, kiln, and oven hot face linings
  • Glass regenerator insulation
  • Heat shields
  • High temperature gaskets and seals
  • Peep door frames and plugs
  • Shapes in ammonia reformers
  • Information provided by Thermal Ceramics

    Data has not been recently verified. Please contact manufacturer for current information.

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Density 0.240 g/cc0.00867 lb/in³
    Loss On Ignition 7.0 - 9.0 %7.0 - 9.0 %
     
    Mechanical PropertiesMetricEnglishComments
    Modulus of Rupture 0.000758 GPa0.110 ksi
    Compressive Yield Strength 0.210 MPa30.5 psiat 5% deformation
     0.280 MPa40.6 psiat 10% deformation
     
    Thermal PropertiesMetricEnglishComments
    Thermal Conductivity  0.0648 W/m-K
    @Temperature 260 °C
    0.450 BTU-in/hr-ft²-°F
    @Temperature 500 °F
     0.0965 W/m-K
    @Temperature 538 °C
    0.670 BTU-in/hr-ft²-°F
    @Temperature 1000 °F
     0.146 W/m-K
    @Temperature 816 °C
    1.01 BTU-in/hr-ft²-°F
    @Temperature 1500 °F
     0.215 W/m-K
    @Temperature 1090 °C
    1.49 BTU-in/hr-ft²-°F
    @Temperature 2000 °F
    Melting Point 1760 °C3200 °F
    Maximum Service Temperature, Air 1430 °C2600 °F
    Shrinkage  0.30 %
    @Temperature 816 °C,
    Time 86400 sec
    0.30 %
    @Temperature 1500 °F,
    Time 24.0 hour
     0.30 %
    @Temperature 982 °C,
    Time 86400 sec
    0.30 %
    @Temperature 1800 °F,
    Time 24.0 hour
     0.60 %
    @Temperature 1090 °C,
    Time 86400 sec
    0.60 %
    @Temperature 2000 °F,
    Time 24.0 hour
     0.70 %
    @Temperature 1200 °C,
    Time 86400 sec
    0.70 %
    @Temperature 2200 °F,
    Time 24.0 hour
     0.80 %
    @Temperature 1320 °C,
    Time 86400 sec
    0.80 %
    @Temperature 2400 °F,
    Time 24.0 hour
     1.0 %
    @Temperature 1370 °C,
    Time 86400 sec
    1.0 %
    @Temperature 2500 °F,
    Time 24.0 hour
     1.4 %
    @Temperature 1430 °C,
    Time 86400 sec
    1.4 %
    @Temperature 2600 °F,
    Time 24.0 hour
     
    Component Elements PropertiesMetricEnglishComments
    Al2O3 51 %51 %
    Other 7.0 - 9.0 %7.0 - 9.0 %
    SiO2 49 %49 %

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    Morgan Advanced Ceramics Kaowool 2600 Organic RCF Vacuum Formed Thermal Ceramic

    CTHERM181 / 2501

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.