MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Covestro Makrolon® 4/10-6 Multi UV sheet, 10 mm Polycarbonate
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: Profile overview Makrolon® multi UV sheet is a family of structured polycarbonate sheet products that offer superior solutions for a wide range of interior finish, glazing, roofing, and cladding applications.

Features and benefits include:

  • Over 250 times more impact resistant than glass–withstands hail storms and breakage during transport and installation
  • Excellent thermal insulation for energy savings
  • High light transmission clear or reduced light transmission tints allow for controlled daylighting
  • Lightweight and easy to install and fabricate–the sheet can be cold-bent during installation
  • Low Flammability–International Building Code Rated
  • Makrolon multi UV sheet is offered with a ten (10) year Limited Product Warranty against breakage and weather resistance
Applications: Industrial buildings, sports arenas, greenhouses, bus shelters, car ports, sunrooms, covered walkways, swimming pool covers, partition walls, facades, roofing, skylights, and lightweight signage

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesMetricEnglishComments
CTE, linear 67.5 µm/m-°C37.5 µin/in-°F
Insulation R Value 2.32.3[hr•ft2•°F / BTU]
 
Optical PropertiesMetricEnglishComments
Yellow Index  2.0 %
@Time 7.20e+6 sec
2.0 %
@Time 2000 hour
after UV exposure
 2.5 %
@Time 3.60e+7 sec
2.5 %
@Time 10000 hour
after UV exposure
 3.0 %
@Time 2.16e+7 sec
3.0 %
@Time 6000 hour
after UV exposure
Transmission, Visible 61 %61 %Opal
 68 %68 %Clear
 
Descriptive Properties
U-value0.44[BTU/hr•ft2•°F]

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Makrolon® AR sheet Polycarbonate
Covestro Makrolon® GP Matte sheet Polycarbonate
Covestro Makrolon® GP Pebble sheet Polycarbonate
Covestro Makrolon® GP Prismatic sheet Polycarbonate
Covestro Makrolon® GP-V Matte sheet Polycarbonate

PCOVEST0847 / 202630

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.