MBA Polymers EvoSource™ 4535 Recycled ABS
Categories:
Polymer
;
Renewable/Recycled Polymer
;
Thermoplastic
;
ABS Polymer
;
Acrylonitrile Butadiene Styrene (ABS), Molded
Material Notes:
A UL-HB recognized, easy flowing, post-consumer recycled acrylonitrile-butadiene-styrene copolymer for general use. Available in standard grey (reference 70/15) and standard black (reference 90/04).
Information provided by MBA Polymers.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.06
g/cc
0.0383
lb/in³
MBA Method
Melt Flow
22
g/10 min
@Load 10.0 kg,
Temperature 220 °C
22
g/10 min
@Load 22.0 lb,
Temperature 428 °F
ISO 1133
Mechanical Properties
Metric
English
Comments
Tensile Strength, Yield
41.0
MPa
5950
psi
ISO 527-2/50
Tensile Modulus
2.30
GPa
334
ksi
ISO 527-2/1
Flexural Modulus
2.25
GPa
326
ksi
ISO 178/2
Izod Impact, Notched (ISO)
15.0
kJ/m²
7.14
ft-lb/in²
180/1A
Charpy Impact, Notched
1.40
J/cm²
6.66
ft-lb/in²
ISO 179/1eA
Electrical Properties
Metric
English
Comments
Volume Resistivity
1.00e+17
ohm-cm
1.00e+17
ohm-cm
ASTM D257
Hot Wire Ignition, HWI
7.0
-
15
sec
@Diameter 1.50 - 2.80 mm
7.0
-
15
sec
@Diameter 0.0591 - 0.110 in
ASTM D 3847
High Amp Arc Ignition, HAI
60
-
120
arcs
@Diameter 1.50 - 2.80 mm
60
-
120
arcs
@Diameter 0.0591 - 0.110 in
UL 746 D
Thermal Properties
Metric
English
Comments
Vicat Softening Point
90.0
°C
194
°F
ISO 306/B50
Flammability, UL94
HB
@Diameter 1.50 - 2.80 mm
HB
@Diameter 0.0591 - 0.110 in
UL 94 HB
Processing Properties
Metric
English
Comments
Melt Temperature
200
-
220
°C
392
-
428
°F
Range, Extrusion
210
°C
410
°F
Recommended Extrusion
210
-
250
°C
410
-
482
°F
Range, Injection Molding
240
°C
464
°F
Recommended, Injection Molding
Mold Temperature
40.0
-
60.0
°C
104
-
140
°F
Range
50.0
°C
122
°F
Recommended
Drying Temperature
80.0
°C
176
°F
Dry Time
3.00
-
4.00
hour
3.00
-
4.00
hour
Moisture Content
0.050 - 0.10 %
0.050 - 0.10 %
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
PMBAP9803 / 282926
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.