MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Superior Flux Superior CCF-2 Centrifugal Casting Flux
Categories: Metal; Nonferrous Metal; Solder/Braze Alloy

Material Notes:
  • Specially formulated for horizontal centrifugal casting machines
  • Protects against oxide formation on metals during casting.
  • Crucial for bonding of dissimilar alloys in centrifugal casting
Description: Superior CCF-2 is a specially formulated flux for the needs of centrifugal casting. This flux consists of a proprietary blend of inorganic chemicals that protects molten metals from oxidation during the casting process. The prevention of oxide formation is instrumental for the joining of dissimilar metals during the casting process. Superior CCF-2 is active in the temperature range of 1700° – 2300°F (925° - 1260°C).

Applications: Superior CCF-2 is funneled into the barrel in accordance with the horizontal centrifugal casting application. The specific amount of product used is gauged according to the size of the barrel and other considerations, such as the particular alloys being cast and the temperature achieved on the inside of the barrel. The active temperature range of Superior CCF-2 is 1700° – 2300°F (925° - 1260°C).

Information provided by Superior Flux

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
pH 4.25 - 5.754.25 - 5.75Dilute, 10.6%
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 925 - 1260 °C1700 - 2300 °FActive Range
 
Processing PropertiesMetricEnglishComments
Shelf Life 2.00 Month2.00 Month
 
Descriptive Properties
ColorOff-White
FormPowder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Johnson Matthey Nickelbraze™ HTN7 Nickel Based Brazing Filler Metal
Materion Silseal® 250 Silver-Copper Brazing Alloy
Kennametal Stellite Deloro® 30 Nickel Alloy
Johnson Matthey Silver-flo™ 56 Cadmium Free Silver Brazing Paste
Johnson Matthey Nickelbraze™ HTN6 Nickel Based Brazing Filler Metal

NSFLUX114 / 185798

solder replacement adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.