SiLK™ I300 560 is designed for easy integration and extendibility, and its formulations offer a robust feature set. High thermal stability and fracture toughness means SilK™ I300 560 is compatible with standard IC processing tools in todays fabrications. SiLK™ I300 560 is fluorine-free, thus is compatible with Ti and Ta barrier materials. Information provided by Dow |