MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
KaMin Lithosperse® NextGen Clay
Categories: Ceramic; Clay

Material Notes: Lithosperse® NextGen is a surface enhanced clay for use in heat-set and sheet-fed inks. It is designed to replace ink resin and ink oil with minimal impact on key ink properties such as ink gloss and ink density.

Industry: Ink

Uses: Lithographic/Offset, Sheetfed, Web Offset Heatset, Web Offset Coldset

Information provided by KaMin LLC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Brightness 84 %Reflectance (TAPPI)
Moisture Absorption at Equilibrium <= 2 %As Produced
 
Descriptive Properties
CAS Number1332-58-7
Crystalline Silica (quartz)<0.1%
Physical FormDry
Shipping PointMacon, GA

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Imerys ImerPlast™ 10WPCT Recycled Polyolefin Resin
Imerys ImerPlast™ 10WPC Recycled Polyolefin Resin
Imerys Ewing™ Kaolin
Dow HS II BASE & 10:1 CLAY CATALYST
Cresset Powers Cress-Alon™ NE6040-ST 4% Nano Clay Loaded, 6.0 r.v. Super Tough Grade Nylon 6, Dry As Molded

CKAMAN900 / 178371

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.