LEXAN 925AU Polycarbonate (PC) is an injection moldable non-halogenated, unfilled transparent flame retardant grade with medium flow. It is UV stabilized and has an MVR of 13 (300°C/1.2kg) and a UL94 V0@3mm, and is available in various color options.Information provided by SABIC |