MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

(Viewing data as-entered. Click here to return)
Cartridge Brass, UNS C26000 (260 Brass), OS035 Temper flat products
Categories: Metal; Nonferrous Metal; Copper Alloy; Brass

Material Notes: Fair to excellent corrosion resistance. Excellent cold workability; good hot formability.

Applications: radiator cores and tanks, flashlight shells, lamp fixtures, fasteners, locks, hinges, ammunition components, plumbing accessories, pins, rivets.

Test specimen: flat products - 1mm thickness.

Key Words: 70/30 brass, CDA 260, CZ106, ISO CuZn30, CEN CW505L
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 8.53 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell F 68
Hardness, Rockwell 30T 31
Tensile Strength, Ultimate 340 MPa
Tensile Strength, Yield 115 MPa
Elongation at Break 57 %In 50 mm
Modulus of Elasticity 110 GPa
Poissons Ratio 0.375
Fatigue Strength 95.0 MPa
@# of Cycles 1.00e+8
Reverse Bending
Machinability 30 %UNS C36000 (free-cutting brass) = 100%
Shear Modulus 40.0 GPa
Shear Strength 235 MPa
 
Thermal PropertiesOriginal ValueComments
CTE, linear 19.9 µm/m-°C
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.375 J/g-°C
Thermal Conductivity 120 W/m-K
@Temperature 20.0 °C
Melting Point 915 - 955 °C
Solidus 915 °C
Liquidus 955 °C
 
Processing PropertiesOriginal ValueComments
Annealing Temperature 425 - 750 °C
Hot-Working Temperature 725 - 850 °C
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 68.5 - 71.5 %
Iron, Fe <= 0.050 %
Lead, Pb <= 0.070 %
Other, total <= 0.15 %
Zinc, Zn 28.5 - 31.5 %
 
Descriptive Properties
Hall Coefficient28 pV · m/A · T
Velocity of Sound3660 m/sat 20°C

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Cartridge Brass, UNS C26000 (260 Brass), OS100 Temper flat products
Cartridge Brass, UNS C26000 (260 Brass), OS050 Temper flat products, tubing
Cartridge Brass, UNS C26000 (260 Brass), OS070 Temper flat products
Cartridge Brass, UNS C26000 (260 Brass), H01 Temper flat products
Cartridge Brass, UNS C26000 (260 Brass), OS015 Temper flat products

MC26000b5 / 11079

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.