MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

PolyMirae Moplen EP5078 Extrusion Molding Grade Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Extrusion Grade; Polypropylene, Sheet/Thermoforming Grade

Material Notes: Moplen EP5078 is a low fluidity heterophasic copolymer designed for extrusion applications with smooth process ability and high mechanical properties. Main applications are extrusion of film/sheet and Thermoforming for heavy duty applications, lamination film and extrusion blow molding containers. "Moplen" EP5078 is suitable for food contact.

Product Features: No Gel / No Odor Good Stiffness and Impact resistance/ Good Heat resistance/ Good Aesthetic

Typical Applications: Multilayer packaging/ High heat resistance thermoforming tray/Blow Molding for cosmetic & detergents bottles : EBM/Sheet extrusion with high gloss

Information provided by PolyMirae

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ASTM D1505
Melt Flow 0.50 g/10 min
@Load 2.16 kg,
Temperature 230 °C
0.50 g/10 min
@Load 4.76 lb,
Temperature 446 °F
Condition L; ASMT D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 29.4 MPa4270 psiASTM D638
Flexural Modulus 1.37 GPa199 ksiASTM D790
Izod Impact, Notched NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 107 °C225 °FASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Braskem RP 270G Extrusion Blow Molding Polypropylene
Dow DNDA-8350 NT 7 Linear Low Density Polyethylene Resin
Dow DNDA-7340 NT 7 Linear Low Density Polyethylene Resin
Dow DMDA-8940 NT 7 High Density Polyethylene Resin
Dow DMDA-8907 NT 7 High Density Polyethylene Resin

PMIRAF21 / 183242

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.