MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Epoxies, Etc 50-3150 FR Flame Retardant Thermally Conductive Epoxy Resin
Categories: Polymer; Thermoset; Epoxy

Material Notes: Description: 50-3150 FR has been formulated to meet the stringent non-burning requirements of UL94 V-0. 50-3150 FR Black Epoxy with Catalyst 12, Catalyst 190, Catalyst 30 are listed with Underwriter’s Laboratory for passing UL94 V-0. This system offers excellent heat transfer, low shrinkage, and outstanding insulation properties. 50-3150FR with Catalyst 30 has a UL (746B) Relative Temperature Index (RTI) rating of 130°C. 50-3150FR Black with Catalyst 190 passes NASA’s outgassing requirements per ASTM E595-07. Typical applications for 50-3150 FR include potting and encapsulating power supplies, transformers, electric motors, capacitors, batteries, coils, insulators, sensors, devices for intrinsic safety, etc... This system is an excellent choice for applications requiring high thermal conductivity and flame retardancy.

Information provided by Epoxies, Etc

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.60 g/cc
Viscosity 1500 cPMixed with Cat. 150
 2000 cPMixed with Cat. 12
 17000 cPMixed with Cat. 30
 28000 cPMixed with Cat. 190
 60000 cPResin
Linear Mold Shrinkage 0.0020 in/in
Outgassing - Total Mass Loss 0.010 %CVCM
 0.50 %
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 90
Tensile Strength 9850 psi
Compressive Strength 15000 psi
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.50e+15 ohm-cm
Dielectric Constant 5.6
@Frequency 60 Hz
Dielectric Strength >= 485 V/mil
Dissipation Factor 0.015
@Frequency 60 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 14.0 µm/m-°C
Thermal Conductivity 2.16 W/m-K
Maximum Service Temperature, Air 200 °C
Heat Distortion Temperature 155 °C
Minimum Service Temperature, Air -60.0 °C
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PFEPOX052 / 316729

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.