MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Huber Magnifin H-5 TV Magnesium Hydroxide
Categories: Ceramic; Oxide; Magnesium Oxide; Other Engineering Material; Additive/Filler for Polymer

Material Notes: MAGNIFIN H-5 TV is a high-purity magnesium hydroxide surface treated with a special coating. Based on a mineral raw material, the patented process guarantees a regular structure of the crystallite MAGNIFIN H-5 TV is tailor-made for plastic and elastomer applications, e.g. . XLPE, XL-EVA, EPDM, EPM, TPO´s, EVA, PE and represents a halogen free flame retardant with low smoke emission and high thermal stability up to 340°C. During the decomposition process no toxic or corrosive gases are generated. the surface treatment favors the compatibility of filler and polymer matrix and therefore improves the mechanical properties of the compound.

CAS No.: 1309-42-8

EC/EINECS No.: 215-170-3

Information provided by J.M. Huber Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.40 g/cc2.40 g/cc
Bulk Density 0.300 - 0.600 g/cc0.0108 - 0.0217 lb/in³
Brightness >= 96 %
@Wavelength 457 nm
>= 96 %
@Wavelength 457 nm
DR LANGE Whiteness
Moisture Absorption 0.300 %
@Temperature 105 °C
0.300 %
@Temperature 221 °F
when packed
Particle Size 0.70 - 1.0 µm0.70 - 1.0 µmd10, laser diffraction
 1.4 - 2.0 µm1.4 - 2.0 µmd50, laser diffraction
 2.4 - 4.4 µm2.4 - 4.4 µmd90, laser diffraction
 >= 45 µm>= 45 µm<0.1 percent Sieve Residue
Specific Surface Area 2.0 - 6.0 m²/g2.0 - 6.0 m²/gBET
 
Mechanical PropertiesMetricEnglishComments
Hardness, Mohs 2.52.5
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity >= 5000 ohm-cm>= 5000 ohm-cm10% susp. in de-ion water
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.56 - 1.581.56 - 1.58
 
Component Elements PropertiesMetricEnglishComments
Loss on Ignition(%) 31 %
@Temperature 1200 °C
31 %
@Temperature 2190 °F
 
Descriptive Properties
Content<1 ppmB2O3
 <10 ppmMnO
 <10 ppmCr2O3
 <10 ppmCu
 <50 ppmAl2O3
 <50 ppmFe2O3
 <50 ppmCaO
 <50 ppmNiO
 = 99.8%Mg(OH)2
FunctionalitySmoke Suppression
Market/Application: Building & ConstructionTunnel Construction Cladding
Market/Application: ThermosetsElastomers (Cross-Linked)
Market/Application: Wire and CableWire & Cable Jacketing - Halogen-Free

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

EHUBER785 / 300891

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.