MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
Ensinger Tecaform™ MT Acetal, Medical Grade (POM)
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Homopolymer, Unreinforced

Material Notes: TECAFORM® MT is Ensinger's specially formulated medical grade acetal. The material is resistant to multiple cleaning and disinfection agents, and to a number of solvents. It can be steam sterilized by the medical industry's usual methods, and will maintain good strength, stiffness, and dimensional stability. the material feedstock meets the requirements specified by the FDA, and its code of federal regulations, CFR 21. It has also been fully assessed for biocompatibility according to US Pharmacopeia (USP) Class VI and ISO 10993.
  • Made from FA compliant resin
  • Tested for biocompatibility in compliance with USP Class VI
  • Tested for Cytotoxicity and compliance according to ISO 10993
  • Easily machinable
while used for a great number of medical applications, TECAFORM MT is particularly suited for use as sizing trials in knee, hip and shoulder replacement procedures.

Information provided by Ensinger

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.41 g/ccASTM D792
Density 0.0509 lb/in³ASTM D792
Moisture Absorption at Equilibrium <= 0.30 %50%RH; ASTM D570
Water Absorption at Saturation 0.50 %ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 1890 psi1% elongation after 1000hr
 7980 psiASTM D638
Elongation at Yield 30 %ASTM D638
Rupture Strength 5800 psi
@Time 3.60e+6 sec
Tensile Modulus 305 ksi1mm/min; ASTM D638
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cmIEC 60093
Surface Resistance 1.00e+14 ohmIEC 60093
Dielectric Constant 3.5
@Frequency 100000 Hz
IEC 250
Dissipation Factor 0.0030IEC 250
 
Thermal PropertiesOriginal ValueComments
CTE, linear 55.0 µin/in-°F
@Temperature 22.8 - 55.0 °C
ASTM E831
Melting Point 320 °FASTM D3418
Maximum Service Temperature, Air 212 °Flong term
Deflection Temperature at 1.8 MPa (264 psi) 230 °FASTM D648
Glass Transition Temp, Tg -76.0 °FASTM D3418
Flammability, UL94 HB
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.
USP Class VI Yes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Delrin Delrin® 500P BK602 POM
Ensinger Delrin® 150 Homopolymer Acetal (POM)
Overview of materials for Acetal Copolymer, Unreinforced
Avient Trilliant™ HC THC-02 1200 IL Natural Polyamide 66 (Nylon 66)
BASF Ultraform® H 2320 006 Q600 POM

PENSIN094 / 122204

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.