Dexflex 1066LS-UV T1 C16001 is a thermoplastic olefinic elastomer (TPO) used for automotive exterior applications that require excellent low-temperature toughness in injection molded parts. Product is available as a customized color matched, pellet form. This grade is delivered in C16001 color version. Status: Commercial - Active Availability: Asia-Pacific Application: Exterior Automotive Applications Market: Automotive Processing Method: Injection Molding Attribute: Low Temperature Toughness Information provided by LyondellBasell. |