MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Phillips 66 32 Super Hydraulic Oil
Categories: Fluid; Lubricant

Material Notes: Description: Conoco Super Hydraulic Oil is a high-quality antiwear hydraulic fluid formulated from premium Conoco hydrocracked base stocks to provide superior water separation, antiwear protection, rust and corrosion inhibition, oxidation resistance and thermal stability. Super Hydraulic Oil is recommended for use in a variety of high-pressure mobile and stationary hydraulic systems utilizing vane, piston or gear pumps, especially where water contamination is a frequent occurrence. Super Hydraulic Oil has been tested and formally approved by Denison Hydraulics in accordance with its premium HF-0 requirements. Super Hydraulic Oil also has been formally approved by Cincinnati Milacron under specifications P-68 (ISO 32), P-70 (46) and P-69 (68). Super Hydraulic Oil exceeds Vickers M-2950-S, Vickers I-286-S and U.S. Steel 127 and 136 requirements. Super Hydraulic Oil is available in a variety of viscosity grades, including two multiviscosity (MV) grades for low temperature operation. Super Hydraulic Oil MV22 and MV32 are high-viscosity index products with exceptionally low pour point and superior low temperature pumpability. Super Hydraulic Oil MV22 and MV32 can be used year-round in hydraulic systems in virtually all climates.

Information provided by ConocoPhillips.

Phillips 66 Lubricants was spun-off from ConocoPhillips in 2012.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.862 g/cc0.0311 lb/in³
Viscosity Measurement 103103Viscosity Index
Saybolt Viscosity at 100°F 165 SUS165 SUS
Saybolt Viscosity at 210°F 44 SUS44 SUS
Kinematic Viscosity at 40°C (104°F) 31 cSt31 cSt
Kinematic Viscosity at 100°C (212°F) 5.4 cSt5.4 cSt
Oxidative Stability 5500 hour5500 hour
ASTM Color 0.500.50
 
Mechanical PropertiesMetricEnglishComments
Four Ball Wear 0.450 mm0.0177 in
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 35.0 kV/mm889 kV/inNo thickness given.
 
Thermal PropertiesMetricEnglishComments
Pour Point -37.2 °C-35.0 °F
Flash Point 216 °C420 °F
 
Descriptive Properties
Emulsion Characteristics (40-40-0)10 minutes
FZGPass 10 Stages
FZG Pass10

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow UCON™ LB-65 Fluids and Lubricants
Anderol ANDEROL® FGH 22 Synthetic Food Grade Hydraulic Fluid, ISO 22
Anderol ANDEROL® FGC 5 Fluid, Synthetic Mechanical Seal Fluid ISO 22
Phillips 66 Syncon® 22 Synthetic AW Hydraulic Fluid 22
ExxonMobil SpectraSyn™ 2 Polyalphaolefin (PAO) Fluid

WCON157 / 75194

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.