NP130 is a woven glass fabric combined with halogenated epoxy resin system. NP130 is produced to printed circuit board quality standards. It is flame retardant, and meets the requirements of MIL-I-24768/27, Type GEE-F.Information provided by Norplex-Micarta |
Glass Fiber, Epoxy, Micarta, NEMA FR-4, ASTM D709 Type IV Grade FR-4, MIL-I-24768/27 GEE-F, IPC 4101/21 |