MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
SEKISUI SPI KYDEX® 7115 Lumina™ PVC/PMMA
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Vinyl (PVC)

Material Notes: KYDEX® 7115 Lumina™ is a PVC/PMMA product that allows light to pass through the material, while silhouettes are still visible. KYDEX® Lumina™ meets stringent FAA compliance for heat release and smoke density. The product allows design freedom in aircraft interiors with our Infused Imaging™ technology to diffuse or disperse light to create effects. KYDEX® Lumina™ has contact clarity: one cannot see through it unless it is illuminated from behind or in a well-lit space.

KYDEX® Lumina™ is designed for backlit panels and decorative accents in aviation interiors. It meets flammability and smoke development requirements outlined in Federal Aviation Regulations (FAR) 25.853 paragraph (a) and (d).

Suggested Application:

  • Privacy screens
  • Class dividers
  • Compartment doors
  • Galley and bar space accents
  • Lavatory fixtures
  • Light diffusers
  • Backlit décor
Features:
  • Increases design freedom for backlit panels and accents
  • Expanded design options with Infused Imaging™ technology
  • Meets the stringent requirements of FAR 25.853 in all thicknesses
  • Excellent fabrication and formability characteristics
  • Resistant to chemical reagents and cleaners commonly used within aviation interiors
  • Available in P3 - Velour Matte texture

Information provided by SEKISUI KYDEX, LLC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.47 g/ccASTM D792
Water Absorption 0.0600 %
@Time 86400 sec
ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 112ASTM D785
Tensile Strength 46.8 MPaASTM D638
Tensile Modulus 3385 MPaASTM D638
Flexural Strength 77.2 MPaASTM D790
Flexural Modulus 3450 MPaASTM D790
Compressive Yield Strength 66.7 MPaASTM D695
Compressive Modulus 3847 MPaASTM D695
Bearing Yield Strength <= 230.3 MPaASTM D953
 37.6 MPa
@Strain 4.00 %
ASTM D953
Poissons Ratio 0.405ASTM D638
Shear Strength 52.6 MPaASTM D732
Gardner Impact 49.1 JDrop Dart Impact, GE; ASTM D5420
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 18.3 kV/mmoil; ASTM D149
 
Thermal PropertiesOriginal ValueComments
CTE, linear 55.6 µm/m-°CASTM E831
Deflection Temperature at 1.8 MPa (264 psi) 73.7 °Cannealed; ASTM D648
 
Descriptive Properties
Vertical BurnPass60 and 12 sec; FAR 25.853(a)(i) and FAR 25.853(a)(ii)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSEKIS516 / 325256

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.