Aquastik™ polychloroprene latexes have been designed for the adhesives industry. They provide an environmentally friendly alternative to solvent-borne systems. This grade features mechanical stability and acid functionality. 47% Solids. Main uses are in adhesives, coatings, and bindings. Initial pH is 7. Low gel polymer type. PVOH emulsifying agent. Very slow crystallization rate. Information provided by DuPont Dow Elastomers. |