MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Thermoseal

Klinger Thermoseal ML-S723 Styrene-Butadiene Gasketing
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Thermoseal ML-S723 is a controlled-swell gasket material intended for heavy-duty applications. ML-S723's blended styrene butadiene and natural rubber binder provides exceptional sealability and conformability with low creep relaxation. Thickness increase, in the presence of oils and fuels, aids the sealing of irregular flange surfaces. Its unique Multi-Layer Technology structure provides exceptional low flange pressure sealability with exceptional torque retention. Multi-Layer Technology sheet products consist of a reinforced high density core with conformable sealing layers on each side. Typical applications include diesel engine oil pan gaskets and gear plate and rear seal carrier gaskets with intermittent operating temperatures up to 350° F (177° C).

Information provided by Thermoseal Inc.

Vendors: Thermoseal Inc. is the exclusive North American producer of Klinger Fluid Sealing products, including popular lines: Sealex, Klingersil and Topchem and our new Performance Technology Group of products. Visit us at Thermosealinc.com or call 1-800-990-7325 to speak with a fluid sealing specialist.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.60 g/cc0.0578 lb/in³ASTM F 1315
Thickness 1590 microns62.5 mil
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Inert 177 °C350 °F
 
Descriptive Properties
Compressibility0.15ASTM F36J
Creep Relaxationmax. 35%1/32", ASTM F38B
Pressure Limitmax. 435 psi
Recoverymax. 40%ASTM F36J
Sealability<0.2 ml/hrASTM F37
Thickness Increase0-10%after immersion in ASTM oil #1, 5hrs @ 149°C, ASTM F146
 0-15%after immersion in Fuel A, 5hrs @ 23°C, ASTM F146
 30-40%after fluid immersion, oil IRM 903: 5h/149°C, ASTM F146
Weight Increasemax. 35%after immersion in Fuel B, 5hrs @ 23°C, ASTM F146

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTHERM954 / 192642

Thermoseal

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.