System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Taiwan PU Corporation TPUI-E80 General Grade, Injection Molding Polyester Base TPU
Categories:
Polymer
;
Thermoplastic
;
Elastomer, TPE
;
Polyurethane, TP
;
Thermoplastic Polyurethane (TPUR), Polyester Grade
Material Notes:
Thermoplastic Polyurethane (TPU), General Grade, Polyester Base, Injection Molding
Information provided by Taiwan PU Corporation.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Mechanical Properties
Original Value
Comments
Hardness, Shore A
80
Tensile Strength at Break
31.38
MPa
Elongation at Break
800 %
100% Modulus
0.00540
GPa
@Strain 100 %
300% Modulus
0.00780
GPa
@Strain 300 %
Resilience
45
%, Impact Resilience
Taber Abrasion, mg/1000 Cycles
40
Processing Properties
Original Value
Comments
Feed Temperature
170
°C
Middle Barrel Temperature
175
°C
Compress zone
Front Barrel Temperature
180
°C
Metering zone
Adapter Temperature
185
°C
Die Temperature
365
°F
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Taiwan PU Corporation TPUI-ED71 General Grade, Injection Molding Polyester Base TPU
Taiwan PU Corporation TPUI-ED64 General Grade, Injection Molding Polyester Base TPU
Taiwan PU Corporation TPUI-E98 General Grade, Injection Molding Polyester Base TPU
Taiwan PU Corporation TPUI-E90 General Grade, Injection Molding Polyester Base TPU
Taiwan PU Corporation TPU-E90 General Grade, Extrusion Molding Polyester Base TPU
PTPU21 / 70877
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.