Description: Dymalink® 708 is a solid dimethacrylate for use in peroxide cured elastomers where enhanced adhesion and dymamic properties are needed. Product Highlights / Performance Properties: - Adhesion promotion
- Peroxide curable
- Excellent dynamic properties
- Abrasion resistance
- High hardness
- High tensile strength
- Improved hot tear strength
- Improved adhesion
Suggested Applications: - Adhesives
- Rubber
- Plastics
Information provided by Cray Valley |