MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Shanghai Potomer LS-22 Acrylic Impact Modifier
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Product property: Fast fusions, good gloss

Brief: LS series Impact Modifier is weatherability Acrylic Impact Modifier used in rigid PVC products. It is a “core – shell” structure modifier with cross-linked poly butyl acrylic as core and graft methyl methacrylate as shell. It not only can improve impact proof performance of the product, but also can increase the surface gloss of the product, especially the weatherability of the product. It is especially suitable for outdoor products and broadly used in PVC profiles, sheets, boards, pipes, pipe fitting etc.

Product Advantage: Compare to CPE and other impact modifiers, LS series AIM have the following advantages:
(1). Imparts excellent low-temperature impact resistance
(2). Excellent weatherability
(3). Improve product surface gloss greatly
(4). Wide processing range for high speed extrusion

Information provided by Shanghai Potomer International Trade Co., Ltd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.400 - 0.550 g/cc0.400 - 0.550 g/cc
Volatiles <= 1.0 %<= 1.0 %
Particle Mesh Size 40 Mesh40 Mesh>98% passing
 
Descriptive Properties
Color/AppearanceWhite flowing powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSPOTOM010 / 284456

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.