MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Baystar™ CD-492 High Density Polyethylene Pipe Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Pipe Grade

Material Notes: Characteristics:
  • Bimodal molecular weight distribution
  • Excellent processing and melt strength
  • Excellent stress crack resistance
  • Meets material requirements for ASTM F2160
Applications:
  • Conduit
  • Corrugated pipe
  • Profile extrusion

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.949 g/cc0.0343 lb/in³ASTM D-792
ESCR 10% Igepal® >= 192 hour>= 192 hourF10 condition B; ASTM D-1693
Melt Flow 0.300 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.300 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D-1238
High Load Melt Index 25 g/10 min
@Load 21.6 kg,
Temperature 190 °C
25 g/10 min
@Load 47.6 lb,
Temperature 374 °F
ASTM D-1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 63.063.0ASTM D-2240
Tensile Strength, Yield 24.8 MPa3600 psiASTM D-638
Elongation at Break >= 600 %>= 600 %ASTM D-638
Tensile Modulus 0.848 GPa123 ksiASTM D-638
 
Thermal PropertiesMetricEnglishComments
Melting Point 131 °C268 °FASTM D-3417

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBAYST806c / 323924

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.