MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Lubrizol ESTANE® 58141 Ester Based Thermoplastic Polyurethane  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Polyester Grade

Material Notes: Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability in a flexible thermoplastic elastomer system that is easy to process in a wide range of equipment. The Estane® TPU portfolio of products offers high performance polyester - and polyether - based resins and compounds in a broad range of hardnesses to meet a variety of application needs.

Benefits of Estane® TPU:

  • Outstanding Abrasion and Wear Resistance
  • Excellent Low Temperature Flexibility
  • Superior Toughness and Durability
  • Ease of Processing and Manufacturing Flexibility
  • Colorability and Paintability with no adhesion promoter
  • Applications:

    • Film & Sheet
    • Fabric coating & melt coating
    • Wire & Cable
    • Hose, Tube & Profile
    • Custom molding
    • Custom compounding
    • Automotive interior/chassis and exterior painted trim

    Information provided by Noveon, Inc.

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Specific Gravity 1.21 g/ccISO 2781
     
    Mechanical PropertiesOriginal ValueComments
    Hardness, Shore A 96ISO 868
    Hardness, Shore D 49ISO 868
    Tensile Strength, Ultimate 30.0 MPaISO 37
    Elongation at Break 540 %ISO 37
    Tensile Modulus 0.0880 GPaISO 527
    50% Modulus 0.0101 GPa
    @Strain 50 %
    ISO 37
    100% Modulus 0.0117 GPa
    @Strain 100 %
    ISO 37
    300% Modulus 0.0200 GPa
    @Strain 300 %
    ISO 37
    Rebound 35 %ISO 4662
    Tear Strength 100 kN/mwith incision; ISO 34B
     138 kN/mwithout incision; ISO 34B
    Abrasion 45mm3; ISO 4649
    Compression Set 19 %
    @Temperature 22.0 °C,
    Time 252000 sec
    ISO 815
     27 %
    @Temperature 70.0 °C,
    Time 86400 sec
    ISO 815
     
    Thermal PropertiesOriginal ValueComments
    Vicat Softening Point 135 °CA50; ISO 306

    **
    Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

    Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    Users viewing this material also viewed the following:
    Lubrizol ESTANE® 58149 Ester Based Thermoplastic Polyurethane
    Lubrizol Estane® 58070 Thermoplastic Polyurethane
    Lubrizol ESTANE® 58091 Ester Based Thermoplastic Polyurethane
    Lubrizol ESTANE® 5799 Ester Based Thermoplastic Polyurethane
    Lubrizol ESTANE® 5778 Ester Based Thermoplastic Polyurethane

    PNOVEON104 / 55371

    Polyurethane

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.