MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Thermal Ceramics Kao-Tex B-30 1800 Cloth
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: Kao-Tex 1800 Cloth is a flexible, high-silica fabric with outstanding thermal insulation characteristics. Kao-Tex 1800 is 96% SiO2 fabric manufactured by an acid-leaching process. Kao-Tex 1800 is totally inorganic and does not smoke when exposed to heat.

Kao-Tex 1800 is primarily used in hot work such as welding and burning operations. It is also useful for thermal and electrical insulation in stress-relieving. Kao-Tex 1800 is available in a wide variety of fabricated forms including curtains, seals, pads, and hemmed blankets.

Features:

  • Made from high silica yarn
  • Easily sewn and fabricated
  • High strength and flexibility
  • Information provided by Thermal Ceramics

    Data has not been recently verified. Please contact manufacturer for current information.

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Thermal PropertiesMetricEnglishComments
    Melting Point 1650 °C3000 °F
    Maximum Service Temperature, Air 927 °C1700 °F
    Shrinkage 10 %10 %Residual
     
    Component Elements PropertiesMetricEnglishComments
    Al2O3 0.071 %0.071 %
    B2O3 >= 0.016 %>= 0.016 %
    CaO 0.023 %0.023 %
    MgO >= 0.017 %>= 0.017 %
    SiO2 97.85 %97.85 %

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    Thermal Ceramics Kao-Tex Cloth 1000
    Thermal Ceramics Kao-Tex B-30 HT 1900 Cloth
    Thermal Ceramics Kao-Tex A-54 HTS 1900 Cloth
    Thermal Ceramics Kao-Tex A-54 1800 Cloth
    Dow BETAFOAM™ 87120 Polyether / Polyol Blend

    CTHERM306 / 2626

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.