System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Azoty Tarnow™ TARFLEN ST PTFE
(discontinued **)
Categories:
Polymer
;
Thermoplastic
;
Fluoropolymer
;
Polytetrafluoroethylene (PTFE)
;
Polytetrafluoroethylene (PTFE), Molded
Material Notes:
Free-Flowing suspension powder for ram extrusion of rods, pipes and other profiles.
Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Bulk Density
0.600
g/cc
0.0217
lb/in³
Density
2.15
g/cc
0.0777
lb/in³
ISO 1183
Particle Size
800
µm
800
µm
Average
Mechanical Properties
Metric
English
Comments
Hardness, Shore D
58
58
ISO 868
Ball Indentation Hardness
34.0
MPa
4930
psi
ISO 2039-1
Tensile Strength, Yield
20.0
MPa
2900
psi
ISO 527
Elongation at Break
250 %
250 %
ISO 527
Izod Impact, Notched
1.40
J/cm
2.62
ft-lb/in
ISO 180
Electrical Properties
Metric
English
Comments
Volume Resistivity
1.10e+18
ohm-cm
1.10e+18
ohm-cm
IEC 60093
Surface Resistance
4.50e+17
ohm
4.50e+17
ohm
IEC 60093
Dielectric Constant
2.1
2.1
IEC 60250
Dielectric Strength
72.0
kV/mm
1830
kV/in
IEC 60243-1
Dissipation Factor
0.00010
0.00010
IEC 60250
Arc Resistance
420
sec
420
sec
IEC 61621
Comparative Tracking Index
600
V
600
V
IEC 112
Thermal Properties
Metric
English
Comments
CTE, linear
125
µm/m-°C
@Temperature 20.0 °C
69.4
µin/in-°F
@Temperature 68.0 °F
ASTM E 831
Specific Heat Capacity
1.00
J/g-°C
0.239
BTU/lb-°F
Thermal Conductivity
0.250
W/m-K
1.74
BTU-in/hr-ft²-°F
Melting Point
327
°C
621
°F
Flammability, UL94
V-0
V-0
Processing Properties
Metric
English
Comments
Processing Temperature
370
°C
698
°F
Molding
Back Pressure
35.0
-
40.0
MPa
5080
-
5800
psi
Molding Pressure
**
Materials flagged as discontinued (
) are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.
Users of our Advanced Search (registration required) may exclude discontinued materials from search results.
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Azoty Tarnow™ TARFLEN SG-2 PTFE
Azoty Tarnow™ TARFLEN SG-1 PTFE
Covestro Apec® DP9-9354 High-Heat Polycarbonate, Flame-Retardant
Mitsubishi Novaduran® 5010N6-3X Polybutylene Terephthalate
Celanese Celanex® XFR 6842 GF15 PBT, 30% Glass Reinforced
PZAK082 / 72921
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.