MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Plastcom SLOVAMID 6 SGF 30 Polyamide 6, 30% Milled Glass Fiber
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled

Material Notes: Features

PA 6 for injection moulding, chemically strengthened with 30% of milled glass fiber, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-goods industry. Application: grips of electrotools, hobby tools, gears, covers of electric appliances, cooling screws of blowers, electromotors, carrying parts in the automotive industry. Delivered in natural mode and in the full RAL color scale.

Application: Injection Moulding

Information Provided by Plastcom spol. s r.o.

Key Words: PA6
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.33 g/ccSTN 64 0111
Linear Mold Shrinkage 0.0084 cm/cmSTN 64 0808
Linear Mold Shrinkage, Transverse 0.0123 cm/cmSTN 64 0808
Melt Flow 3.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
STN EN ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 110 MPaSTN EN ISO 527-2
Elongation at Break 6.0 %STN EN ISO 527-2
Tensile Modulus 7500 MPaSTN EN ISO 527-2
Flexural Strength 185 MPaSTN EN ISO 178
Flexural Modulus 6400 MPaSTN EN ISO 178
Charpy Impact Unnotched 40.0 kJ/m²
@Temperature -20.0 °C
STN EN ISO 179
 45.0 kJ/m²
@Temperature 23.0 °C
STN EN ISO 179
Charpy Impact, Notched 3.00 kJ/m²
@Temperature -20.0 °C
STN EN ISO 179
 6.00 kJ/m²
@Temperature 23.0 °C
STN EN ISO 179
 
Thermal PropertiesOriginal ValueComments
Melting Point 220 °CDSC; STN EN ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 195 °CSTN EN ISO 75/A
Vicat Softening Point 200 °CB; STN EN ISO 306
Flammability, UL94 HB
Glow Wire Test 650 °CSTN IEC 60695-2-10
 
Processing PropertiesOriginal ValueComments
Melt Temperature 250 - 280 °C
Mold Temperature 70.0 - 90.0 °C
Drying Temperature 80.0 °C
Dry Time 4 hour
Moisture Content 0.15 %STN EN ISO 960
Injection Pressure 70.0 - 120 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Delrin Delrin® 500P BK602 POM
CP-Polymer-Technik Wellamid® 6000 MF 30 HWCP 30% Milled Glass Fiber Nylon 6, Heat Stabilized, Dry
CP-Polymer-Technik Wellamid® 6000 MF 30 HWCP 30% Milled Glass Fiber Nylon 6, Heat Stabilized, Conditioned
CP-Polymer-Technik Wellamid® 6600 MF30 HWCP 30% Milled Glass Fiber Nylon 66, Heat Stabilized, Dry
Delrin Delrin® 500P NC010 POM

PPLACO017 / 106895

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.