MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Cogegum® AFR/920 Polyolefin  (discontinued **)
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes: Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without halogenidric acids evolution; furthermore, toxic and corrosive gases emission and smoke generation are particularly reduced. These characteristics make this compound suitable in all applications where the fire behavior of cable materials is one of the main concerns to be considered in establishing a high safety level in public places. This material complies with RoHS requirements. standard complying - EN 50363-0 M1, M9; EN 50363-7 TI6, TI7; EN 50363-8 TM7; IEC 60502-1 ST8; Cenelec HD 624.7 S1; Cenelec HD 624.6 S1; VDE 0207 HM2, HM4, HM5, HJ2; BS 7655 LTS1, LTS2, LTS3, LTS4; BS 6724; IEC 60092 SHF1; UNE 211002 TIZ1; UNE 21123-4

Additional Information: Tests reported are performed on pressed or extruded specimens Coloring - EVA or PE based masterbatches added at 1.2-1.5% by weight; in order to avoid scotching problems during processing, predrying of colour masterbatch is suggested if moisture absorption occurred during storage (4-6 hours at 50-60°C). Storage - The product must be stored under the following conditions: -- closed and undamaged bags -- ambient temperature not exceeding 35°C -- avoid direct exposure to sunlight and weathering - Product alterations could occur due to extended period of storage - Shelf life: 12 months - Solvay Specialty Polymers accepts no liability of any kind in case the above mentioned conditions are not fulfilled. Packaging - 25 kg moisture-resistant bags on 1375 kg pallet - 1000 kg carton box

Extrusion Notes: Extrusion equipment - standard extruders for thermoplastics equipped with low compression screw (1:1.2-1.4 compression ratio and 20-25 L/D ratio are suggested), and an adequate barrel thermoregulation - don't use screw thermoregulation - filter net: not necessary; in case, use 40-80 mesh/cm² max. Anyway the use of the breaker plate is advisable, in particular using low compression screws

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.43 g/ccASTM D792
ESCR 10% Igepal® >= 1000 hour
@Thickness 3.00 mm,
Temperature 50.0 °C
Condition A, Compression Molded; ASTM D1693
Melt Flow 18 g/10 min
@Load 21.6 kg,
Temperature 190 °C
Internal Method
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 50ISO 868
Tensile Strength at Break 14.3 MPaIEC 60811
Elongation at Break 190 %IEC 60811
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 5.40e+13 ohm-cm
@Temperature 70.0 °C
IEC 60502
 8.10e+14 ohm-cm
@Temperature 20.0 °C
IEC 60502
Insulation Resistivity 200 Megaohm/1000 m
@Temperature 70.0 °C
IEC 60502
 3000 Megaohm/1000 m
@Temperature 20.0 °C
IEC 60502
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 280 °CTemperature Index (Burning); NES 715
Oxygen Index 37 %ASTM D2863
 
Processing PropertiesOriginal ValueComments
Processing Temperature 170 - 180 °CCollar Temperature
Zone 1 130 - 150 °C
Zone 2 150 - 170 °C
Zone 3 160 - 180 °C
Zone 4 170 - 180 °C
Die Temperature 180 - 200 °C
Head Temperature 180 - 190 °C
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 North America
Bending TestPass-25°C; IEC 60811
Calorific Potential18 MJ/kgISO 1716; Upper (gross)
Cold ImpactPassIEC 60811; -25°C
Corrosive Gas in Smoke< 10.0 µS/mmConductivity IEC 60754-2
 pH > 4.30
FeaturesFlame Retardant
 Halogen Free
 Low Smoke Emission
 Low Toxicity
 Self Extinguishing
GenericPolyolefin, Unspecified
Halogenidric Acid Emissions< 0.10%
Heat ShockPassIEC 60811; 150°C
Hot Pressure Test< 50%90°C; max penetration, K=0.6; IEC 60811
Hydrocarbons Immersion Test, 25°C, 4 hr14CEI 20-34/0-1; % Change in Tensile Elongation
 -6CEI 20-34/0-1; % Change in Tensile Strength
Mechanical Properties After Aging in Air Oven, 110°C, 168 hr-15IEC 60811, %Change in Tensile Elongation
 8IEC 60811, %Change in Tensile Strength
Mechanical Properties After Aging in Air Oven, 80°C, 168 hr-17IEC 60811, %Change in Tensile Elongation
 5IEC 60811, %Change in Tensile Strength
RoHS ComplianceRoHS Compliant
SAE 20 Oil Immersion Test, 70°C, 4 hr-11% Change in Tensile Strength
 -6% Change in Tensile Elongation
UsesCable Jacketing
 Low Voltage Insulation
 Wire & Cable Applications
Water Absorption (mg/cm²)1100°C; 24 hr; IEC 60811
Water Immersion Test, 70°C, 168 hr-10% Change in Tensile Elongation
 -13% Change in Tensile Strength

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOL8Y7623 / 135686

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.