MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Dover Chemical EMULAMID FO5DF Diisopropanolamide, Co-Emulsifier / Corrosion Inhibitor
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Emulamid FO5-DF is a DEA-free fatty amide designed for incorporation into most water dilutable metalworking products. Emulamid FO5-DF, in addition to corrosion inhibition, provides enhanced boundary lubricity and metal wetting characteristics to the finished coolant. Also, enhanced hard water stability can be achieved with this product compared to the conventional DEA-containing amides. Emulamid FO5-DF is recommended at treat levels of 5-10% in semi-synthetics and synthetic fluids. Higher treat levels (10-20%) are recommended for water soluble drawing compounds. In these applications, Emulamid FO5-DF produces an elevated viscosity characteristic and high film strength when the finished product is inverted with water (water added to product) prior to the drawing operation. Seasonal variations in raw materials may slightly alter Emulamid FO5-DF’s appearance and sensitivity to cooler temperatures. Under cooler environments, gelling or solidification may occur. Gradual warming of the material will return the product to the typical homogeneous fluid appearance.

Information provided by DoverChem

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.970 g/cc
@Temperature 15.6 °C
Density 8.11 lb/gal
 
Chemical PropertiesOriginal ValueComments
Total Acid Number 4.0[meqHCl/g]
 
Descriptive Properties
AppearanceClear dark amber

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WDOVER124 / 217743

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.